Material | athode | athode | Film |
---|---|---|---|
1 | AL | Ni | PP |
2 | Al partly plated Ni-P (NA) |
Cu plated Ni (NC) |
PE/PP |
3 | Clad Metal (Al/Ni) |
Clad Metal (Al/NC, Al/Cu |
PP/Nonwoven fabric |
Material | athodeathodeFilm | ||
---|---|---|---|
Thickness (§®) | Width (§®) | Material (Cathode/Anode) |
|
Small | 0.08~0.2 | 1~10 | L/NI AL/NC NA/NC |
Medium | 0.1~0.3 | 11~30 | AL/NC NA/NC |
Large | 0.1~0.5 | 31~100 | AL/NC NA/NC |
Extra large | 0.1~0.8 | Over 100 | AL/NC NA/NC |
Item | Standard | Measuring Method |
---|---|---|
Peel Strength |
ASTM D3330 | Put a certain amount of lithium secondary battery electrolyte and Lead Tab in Al Pouch, store it at 80¡É for a certain time, and measure the peel strength of the film with a tensile tester |
Air Tightness |
KS B 0816 | Penetration detection test with the penetrants in the Lead Tab and check the color change with naked eye or microscope |
Bend Test | KS B 0804 | Bending test with 180¡Æ of angle |
Salt Water Spray |
S C IEC 60068-2-11 | Spray 5% NaCl aqueous solution at a certain interval under 35¡É conditions, store it for 24 hours, and check the surface condition. |
Scribe-Grid Test |
ASTM B571 97 | Scratch the metal surface with three or more rectangular grid with strong tool, and attach a special tape, and then check if coating particles get on the tape when detached. |
Visual Inspection |
. | Check the product surface for defects such as chipping, deformation, contamination, rust, scratch, etc. with visual or microscope |
Dimension | Drawing | Check using Vernier calipers or three-dimensional measuring instruments with reference to the dimensions indicated in the design drawing |